The ring spinning system is the oldest spinning system that remains dominant because of the high-quality yarns it produces. Ring spinning has various advantages besides disadvantages.It is the most flexible system from the viewpoints of fibers which can be used and the extent of the yarn counts which can be produced.

The ring spinning system is the oldest spinning system that remains dominant because of the high-quality yarns it produces. Ring spinning has various advantages besides disadvantages.It is the most flexible system from the viewpoints of fibers which can be used and the extent of the yarn counts which can be produced.

Advantages of Ring Spinning

The Ring Spinning System allows various types and lengths of fibers (natural, man-made) to spin on a wide count range from 6 tex to 118 tex
whereas this range is between 17 and 118 tex in rotor spinning. By combing option, the high quality combed yarns which are smoother, brighter and more compact can be produced using the ring system. On the other hand, the ring spinning system has two main problems. The first is low production speed because of frictional contact of ring and traveler, and the yarn tension caused, and the second is high energy consumption that causes high production costs

Following are the advantages of Ring Spinning Process

  • Production of high strength yarns.
  • The spinning of fine count yarns.
  • Proper for special yarns.
  • It is universally applicable (any material can be spun).
  • The know-how for the operation of a machine is well established accessible to everyone.
  • It is flexible as regards quantities (blend and lot size).
  • Since the speeds in drawing section are best controlled, yarn evenness is excellent. But if short fibers are too much, yarn unevenness occurs.
  • Fine yarns can be produced as compared to the open-end system

Disadvantages of Ring Spinning

Following are the disadvantages of choosing Ring Spinning Process

  • Process stages are more numerous. Roving stage exists as an extra process compared to the other systems.
  • Yarn breakages are more numerous as a result of ring traveler friction and yarn air friction. Interruptions, broken ends and piecing up problems exist because of the yarn breakages.
  • The high speed of the traveler damages the fibers.
  • The capacity of the cops is limited.
  • Energy cost is very high.
  • Low production rate.
  • New spinning processes have difficulty in gaining widespread acceptance. Owing to their individual limitations, the new spinning processes are confined to restricted sectors of the market.
  • The ring frame can only survive in the longer term if further success is achieved in automation of the ring spinning process. Also, spinning costs must be markedly reduced since this machine is significant cost factor in a spinning mill.
  • The cost structure in ring spinning mill is shown in the graph.
4 Comments
  1. Arab Basalt Fiber Company says

    Similar to the ring spinning process, the production of BFRP rebar involves several steps. BFRP rebar is crafted from basalt fibers using pultrusion technology, a continuous process starting from raw basalt rock. Initially, basalt rocks undergo crushing, washing, and are then placed into gas-heated furnaces at around 1400 degrees Celsius. The resulting fibers are further processed into straight and bend bars. This intricate process requires the expertise of professionals from esteemed companies such as arabbasaltfiber.com

  2. Jemmy says

    Good to hear this

  3. Arab Basalt Fiber Company says

    Just Like Ring Spinning process, there are few process in making of BFRP rebar. BFRP Rebar is manufactured from Basalt Fiber’s by pultrusion technology which is a continuous process from only raw basalt rock. First, the basalt rocks are crushed, washed, and loaded into a gas-heated furnaces at approximately 1400 degrees Celsius. The produced Fiber’s then processed into straight and bend bars. Only experts from the well renowned company like https://arabbasaltfiber.com/ can work on this.

  4. UTM says

    Visit our Website: https://universaltextilemachinery.com

    Hi…!!!
    I want to write blogs for your website. Kindly give me permission.
    Thank You.

Leave A Reply

Your email address will not be published.